| Place of Origin |
Fujian China (Mainland) |
| Brand Name |
SHIDA |
| Model Number |
TR |
Characteristics: 1.elasticity and appearance of the rubber 2.foggy and shinny surface 3.good feeling of touching and strong elasticity 4.sewing directly and recyclable Natural report: PROPERTIES UNIT VALUE Density g/cm³ 0.98 Abrasion resistance m m³ 250-330 Tensile strength kg/cm² 60.42 Tear strength kg/cm 33.33 Stretching % 890 Hardness A 55-75 Flexion Ciclos >50,000 Operating condition T1=135ºC T2=140ºC T3=145ºC T4=145ºC Open traces presses:60-70Mpa Second rolling:30-40Mpa Third rolling: 35Mpa Feeding presses:110Mpa Back pressure: 20-30Mpa Our TR granules, with better quality than TPR, are applied to production of shoe midsole,outsole,fittings and toys.